濟(jì)南鋁板陽(yáng)極氧化膜如何檢測(cè)?
1、觀察濟(jì)南鋁板http://www.7075lu.com/顏色,已生成氧化膜的純鋁板表面是乳白色,鑄鋁,雜鋁呈灰黑色。未生成氧化膜的表面呈透明的亮白色,有的還附有粉紅或灰黑色的掛霜。
Jinan observed aluminum color, has generated pure aluminum oxide film surface is white, cast aluminum, aluminum miscellaneous grayish black. Did not generate a transparent oxide film surface was bright white, some gray with pink or black frost.
2、測(cè)量濟(jì)南鋁板電阻,已生成氧化膜的檢測(cè)時(shí)有電阻,常壓下不導(dǎo)電,未生成氧化膜的檢測(cè)時(shí)能導(dǎo)電。
Jinan aluminum measuring resistance, the generated oxide film has resistance detected when non-conductive under normal pressure, can be detected when the conductive oxide film is not generated.
3、劃痕,已生成氧化膜的濟(jì)南鋁板表面很硬,用針劃時(shí)打滑,無(wú)劃痕,未生成氧化膜的表面很軟,用針劃時(shí)有阻力和劃痕。
Scratches, Jinan generated aluminum oxide film surface is very hard, when you draw with a needle slipping, no scratches, no surface oxide film is very soft, there is resistance and scratches with a needle scratch.
4、聽(tīng)聲,已生成氧化膜的濟(jì)南鋁板敲打時(shí)會(huì)發(fā)出清脆聲,未生成氧化膜的敲打時(shí)發(fā)出悶聲。
Listen to the sound, it will issue a crisp sound generated when the aluminum oxide film Jinan beat, beat of the oxide film at issue did not generate muffled.
5、對(duì)濟(jì)南鋁板http://www.7075lu.com/進(jìn)行著色檢驗(yàn),已生成氧化膜的在染色溶液中很快可以上色,未生成氧化膜的在染料溶液中染不上色。
Jinan colored aluminum plate test, the generated oxide film may be colored in a dye solution quickly, the oxide film is not generated in the dye solution, dye not color.
公司新聞排行
- 橘皮花紋鋁板的分類與應(yīng)用
- 花紋鋁板在建筑行業(yè)的應(yīng)用
- 鋁板廠家告訴你為什么鋁板表面要進(jìn)行貼膜?
- 濟(jì)南幕墻鋁單板規(guī)格有什么不同
- 濟(jì)南鋁單板幕墻多樣性的類型
- 濟(jì)南外墻鋁單板的創(chuàng)新設(shè)計(jì)與環(huán)保理念
- 鋁板廠家談?wù)勪X板在運(yùn)輸過(guò)程中是如何存放的?
- 濟(jì)南花紋鋁板經(jīng)常被用作外殼材料
- 花紋鋁板怎么去維護(hù)洗刷更干凈而且不傷表層呢
- 鋁板的五種表面處理方法
行業(yè)知識(shí)排行
- 常用鋁板材質(zhì)型號(hào)有哪些?
- 氧化鋁板和普通鋁板如何區(qū)分
- 彩色合金鋁板使用的注意事項(xiàng)
- 濟(jì)南氟碳鋁單板出現(xiàn)漏水問(wèn)題應(yīng)該怎么解決?
- 什么是濟(jì)南鋁蜂窩板,到底好不好?
- 為什么鋁板加工時(shí)需要注意精準(zhǔn)度?
- 如何選購(gòu)好的鋁板
- 通過(guò)看外觀和試手感都能鑒別出濟(jì)南花紋鋁板質(zhì)量好壞
- 解析合金鋁板中各種金屬元素的作用
- 花紋鋁板在使用過(guò)程中要注意哪些問(wèn)題